In situ SEM observation of column-like and foam-like CNT array nanoindentation

Matthew R Maschmann1, Qiuhong Zhang, Robert Wheeler

  • 1Air Force Research Laboratory, Materials and Manufacturing Directorate, AFRL/RX, Wright-Patterson Air Force Base , Ohio 45433, United States.