Curing Methods01:26

Curing Methods

Concrete members with a small surface-to-volume ratio are cured by oiling and moistening the forms before casting the concrete member. These forms can be left in place for a prolonged period to prevent moisture loss, and can be wetted if made of a material suitable for wetting. If the forms are removed early, the concrete member is moistened and covered with polythene sheets to maintain moisture. For large horizontal concrete surfaces exposed to dry weather, a temporary covering is suspended...
Curing of Concrete01:20

Curing of Concrete

The hydration of cement takes place within the water-filled capillary pores. However, environmental elements can disrupt this process by evaporating water from the concrete surfaces. Sealed concrete with a water-cement ratio below 0.5 experiences self-desiccation, leading to water loss. The water loss in concrete is mitigated by curing. This technique involves keeping the concrete saturated to maintain the necessary temperature and moisture conditions, to optimally fill the spaces in the cement...
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
Mortar Joint Deterioration in Masonry01:13

Mortar Joint Deterioration in Masonry

Mortar joint deterioration is a significant concern in masonry structures, with water accumulation in the joints leading to damage from freeze-thaw cycles. The repeated expansion of water during freezing and its melting during thawing develop and propagate cracks in the masonry joints. Eventually, this leads to the spalling of mortar from the joints, loosening masonry units and weakening the structure. The deteriorated mortar joints are also vulnerable to moisture intrusion into the walls.
The...
States of Water01:23

States of Water

Water exists in any one of the three classical states: solid (ice), liquid (water), and gas (steam or water vapor). The state of water depends on i) the intermolecular forces that draw molecules together and ii) the kinetic energy that leads to movements that pull them apart.
Water freezes when the intermolecular forces are greater than the kinetic energy. Unlike most other substances, water is less dense in its solid state than in its liquid state. This is because each water molecule can form...