Related Experiment Video
Updated: Jun 3, 2026

Epitaxial Growth of Perovskite Strontium Titanate on Germanium via Atomic Layer Deposition
Published on: July 26, 2016
Infrared phonon spectroscopy of a compressively strained (001) SrTiO₃ film grown on a (110) NdGaO₃ substrate
Abstract:
Polarized infrared reflectivity was measured between 5 and 300 K on a 17 nm thick, 1.1% compressively strained epitaxial (001) SrTiO(3) film and the orthorhombic (110) NdGaO(3) substrate upon which it was grown. A strong in-plane infrared anisotropy of the NdGaO(3) substrate was observed and polar modes with B(1u)-and a mixture of B(2u) + B(3u)-symmetry were seen. At low temperatures three new modes arose in the 90-130 cm( - 1) range, which we assigned to 4f Nd electronic transitions. The in-plane SrTiO(3) film phonons showed strong stiffening compared to the phonon frequencies of bulk unstrained SrTiO(3), particularly the soft mode, and the in-plane phonon peaks were found to split. No anomalies were detected as a function of temperature in either the infrared response or lattice parameters of the compressively strained SrTiO(3) film, providing an absence of evidence for the out-of-plane ferroelectric phase transition predicted by theory.
Related Concept Videos
IR Spectroscopy: Hooke's Law Approximation of Molecular Vibration
According to Hooke's law, the vibrational frequency is directly proportional to the...
IR Spectroscopy: Molecular Vibration Overview
Stretching vibrations are vibrational motions that occur along the bond line, changing the bond length or distance between two bonded atoms. They are further distinguished as symmetric or asymmetric. In symmetric stretching, the...
IR Frequency Region: X–H Stretching
IR Spectrum Peak Splitting: Symmetric vs Asymmetric Vibrations
Measurements of Strain
IR Frequency Region: Alkene and Carbonyl Stretching
Stretching frequencies are affected by several factors, such as resonance, inductive effects, ring strain, dipole moment, and hydrogen bonding. Consequently, the stretching frequency of the carbonyl double bond varies in...