Atomic layer deposition of organic-inorganic hybrid materials based on saturated linear carboxylic acids
Karina Barnholt Klepper1, Ola Nilsen, Per-Anders Hansen
1Department of Chemistry and Centre for Materials Science and Nanotechnology, University of Oslo, P.O. Box 1033, Blindern, Oslo N-0315, Norway. k.b.klepper@kjemi.uio.no
Abstract:
Atomic layer deposition (ALD) has successfully provided thin films of organic-inorganic hybrid materials based on saturated linear carboxylic acids and trimethylaluminium (TMA). Films were grown for seven carboxylic acids: oxalic, malonic, succinic, glutaric, pimelic, suberic and sebacic acid, i.e. ranging from 2 to 10 carbon atoms in the molecular structure. These processes show exceptionally high growth rates; up to 4.3 nm/cycle for the pimelic acid-TMA system. Quartz crystal microbalance measurements of the growth dynamics indicate that all systems are of a self limiting ALD-type. Nevertheless, temperature dependent growth was observed in several systems. The width of the ALD windows shows correlations with the length of the carbon chains. Fourier transform infrared spectroscopy clearly proved that the deposited films are of a hybrid character, where the carboxylic acids primarily form bidentate complexes, though bridging complexes may also form. All films are X-ray amorphous as deposited. The films were further analyzed by atomic force microscopy for surface roughness and topography, UV-Vis spectroscopy and ellipsometry for optical properties, and the goniometer method for measuring sessile drops for surface wetting properties. Apart from the oxalic and malonic acid-TMA systems, the films are stable in contact with water. The films are generally smooth, transparent and have a refractive index close to 1.5. The complete coverage and accurate growth control offered by the ALD technique is here proven to provide surface-functionalized hybrid materials resembling metal-organic frameworks (MOF), probably as rather dense structures, yet with substantial potential for applications.
Related Concept Videos
Carboxylic Acid Derivatives: Overview
Acid Halides to Carboxylic Acids: Hydrolysis
As shown below, the mechanism involves a nucleophilic attack by water at the carbonyl carbon to form a tetrahedral intermediate. This is followed by the reformation of the carbon–oxygen π bond along with the departure of a halide ion. A final proton transfer step yields carboxylic acid...
Preparation of Carboxylic Acids: Hydrolysis of Nitriles
Reactions of Carboxylic Acids: Introduction
Structures of Carboxylic Acid Derivatives
Carboxylic acid derivatives contain an acyl group attached to a heteroatom such as chlorine, oxygen, or nitrogen. The carbonyl carbon and oxygen are both sp2-hybridized with an unhybridized p orbital.
The three sp2 orbitals of the carbonyl carbon form three σ bonds, one each with the carbonyl oxygen, the α carbon, and the heteroatom, whereas the other two sp2 orbitals of the carbonyl oxygen are occupied by the lone pairs. Further, the unhybridized p...
Preparation of Carboxylic Acids: Overview