Effect of test environment and microstructure on the flexural strength of dental porcelains

Vinicius Rosa1, Paulo Francisco Cesar, Carlos Felipe Sarmento Pereira

  • 1Department of Dental Materials, University of São Paulo, Brazil.

Abstract

Related Concept Videos

Strength of Cement01:20

Strength of Cement

Strength tests for cement are not performed directly on neat cement paste due to difficulty in obtaining consistent, reliable specimens. Instead, cement is typically tested in the form of cement-sand mortar.
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Porosity in Cement Paste01:18

Porosity in Cement Paste

The porosity of concrete is a measure of the void spaces within its structure. These spaces impact its strength and durability significantly. When water and cement interact, a chemical reaction called hydration creates a semi-solid paste. This paste includes combined water, making up approximately 23% of the cement's dry mass, and gel water, which fills minuscule voids known as gel pores, accounting for about 28% of the cement gel volume.
The balance of water to cement in the mix is critical—it...
Flexural Stress01:16

Flexural Stress

When analyzing bending in symmetric members, it's crucial to understand how stresses distribute when subjected to bending moments. This stress distribution is effectively described by applying fundamental mechanics and material science principles, particularly Hooke's Law for elastic materials.
Hooke's Law states that within the material's elastic limits, stress is directly proportional to strain. In a member experiencing a bending moment, the strain at any point is relative to its distance...