Hydrothermal treatment of electric arc furnace dust
Bing-Sheng Yu1, Yuh-Ruey Wang, Tien-Chin Chang
1Institute of Mineral Resources Engineering, National Taipei University of Technology, Taipei 106, Taiwan, ROC.
Abstract:
In this study, ZnO crystals were fabricated from electric arc furnace dust (EAFD) after alkaline leaching, purification and hydrothermal treatment. The effects of temperature, duration, pH, and solid/liquid ratio on ZnO crystal morphology and size were investigated. Results show a high reaction temperature capable of accelerating the dissolution of ZnO precursor, expediting the growth of 1D ZnO, and increasing the L/D ratio in the temperature range of 100-200°C. ZnO crystals with high purity can also be obtained, using the one-step hydrothermal treatment with a baffle that depends on the different solubility of zincite and franklinite in the hydrothermal conditions.
More Related Videos
Related Concept Videos
Microbial Leaching
Acid Mine Drainage
Biological Treatment of Effluent and Waste Water
Sample Preparation for Analysis: Advanced Techniques
Acid digestion with strong acids is commonly used to dissolve inorganic materials that are insoluble (do not dissolve) in water. This method can be useful for...