Transverse mechanical properties of collagen fibers from nanoindentation

Katerina E Aifantis1, Sanjiv Shrivastava, Gregory M Odegard

  • 1Laboratory of Mechanics, Aristotle University of Thessaloniki, 54-124 Thessaloniki, Greece. kaifanti@mtu.edu

Related Concept Videos

Deformations in a Transverse Cross Section01:21

Deformations in a Transverse Cross Section

When a material is subjected to uniaxial stress, it elongates or contracts in the direction of the applied force, and also undergoes changes in the perpendicular directions. This behavior is crucial for understanding how materials behave under stress and is governed by mechanical properties such as Poisson's ratio v, which measures the ratio of transverse strain to axial strain.
As the material stretches, it expands or contracts in orthogonal directions to the load. This phenomenon varies...
Normal Strain under Axial Loading01:20

Normal Strain under Axial Loading

Normal strain under axial loading is an important concept in the field of mechanics of materials. Axial loading implies the application of a force along the axis of a material, like a column or bar. This force can either compress or stretch the material. In the context of axial loading, normal strain is the deformation experienced by the material in the direction of the loading force. It's calculated as the change in length divided by the original length of the material. This unitless ratio...
Fibril-associated Collagen01:11

Fibril-associated Collagen

Fibril-associated collagens are a type of collagens present in the extracellular matrix with interrupted triple helices or FACIT (Fibril-associated collagens interrupted triple-helices). FACIT help connect and attach the collagen fibrils with each other as well as with other proteins of the extracellular matrix.
For example, the type II collagen fibrils in cartilage have covalently bound type IX fibril-associated collagens at regular intervals. Other types of fibril-associated collagens are...