Purpose:
Glass ionomer sealants (GISs) are promoted in pediatric dentistry for their moisture-friendly properties. This study's purpose was to investigate the marginal leakage of a glass ionomer sealant (Fuji Triage) under different moisture environments.
Methods:
Eighty extracted teeth were distributed into 4 groups: (1) control; (2) saliva contamination with 1-second air-thinning; (3) saliva contamination with 10 seconds of air-drying; and (4) saliva contamination with reconditioning. Sealants were placed after contamination. All extracted teeth underwent thermocycling followed by 1% methylene blue dye and distilled water wash. All extracted teeth were then sectioned buccolingually into 3 cross-sections and examined at 60X under a stereomicroscope. Microleakage was assessed using a dye penetration scoring system (score=0-3). Data were analyzed with Kruskal-Wallis and Mann-Whitney tests.
Results:
The control group showed significantly lower marginal leakage than the other 3 groups (P<.02). There was no statistically significant difference among the 3 contaminated groups (P>.34).
Conclusions:
Fuji Triage sealant had the least marginal leakage under a moisture-controlled environment. When saliva was introduced during the application of the material, microleakage significantly increased. When contamination occurred, 1-second air-thinning of the saliva, 10-second air-drying of the saliva, or reconditioning before sealant application did not show a difference in decreasing microleakage.
Related Concept Videos
Microcracking in Concrete
Permeability of Concrete
Waterproofing and Anti-Bacterial Admixtures in Concrete
Waterproofing admixtures render concrete hydrophobic,...
Porosity in Cement Paste
The balance of water to cement in the mix is critical—it...
Bleeding in Fresh Concrete
Bleeding can cause several issues in the concrete structure. Sometimes, the rising water gets trapped beneath large aggregate...