Nanomechanical properties of α-synuclein amyloid fibrils: a comparative study by nanoindentation, harmonic force

Kim Sweers1, Kees van der Werf, Martin Bennink

  • 1Nanobiophysics Group, MESA+ Institute for Nanotechnology, Faculty of Science and Technology, University of Twente, Enschede, The Netherlands. k.k.m.sweers@utwente.nl.