Heterogeneous nucleation and growth of the β(Ti) phase in the Ti-Al system-experiments and model calculations

Daniel Gosslar1, Christian Hartig, Robert Günther

  • 1Institute of Materials Science and Technology, Hamburg University of Technology, Eissendorfer Straße 42, D-21073 Hamburg, Germany.

Related Concept Videos

Phase Diagrams of Ternary Systems01:28

Phase Diagrams of Ternary Systems

Consider a ternary system, which is composed of three components: water (W), ethanoic acid (E), and trichloromethane (T). Here, Ethanoic acid (E) is fully miscible with both water (W) and trichloromethane (T), meaning it can mix entirely with either of them. However, water and trichloromethane have partial miscibility, meaning they can only mix to a certain extent, beyond which two separate phases will form.The phase diagram of a ternary system is represented as an equilateral triangle, where...
Ziegler–Natta Chain-Growth Polymerization: Overview01:17

Ziegler–Natta Chain-Growth Polymerization: Overview

Ziegler–Natta polymerization is another form of addition or chain‐growth polymerization used for synthesizing linear polymers over branched polymers. The catalyst used for polymerization is the Ziegler–Natta catalyst, named after Karl Ziegler and Giulio Natta, who developed it in 1953. This catalyst is an organometallic complex of titanium tetrachloride and triethyl aluminum, with the active form of the catalyst being an alkyl titanium compound. Using the Ziegler–Natta catalyst, high molecular...
Phase Transitions: Melting and Freezing02:39

Phase Transitions: Melting and Freezing

Heating a crystalline solid increases the average energy of its atoms, molecules, or ions, and the solid gets hotter. At some point, the added energy becomes large enough to partially overcome the forces holding the molecules or ions of the solid in their fixed positions, and the solid begins the process of transitioning to the liquid state or melting. At this point, the temperature of the solid stops rising, despite the continual input of heat, and it remains constant until all of the solid is...