Luminescence from single CdSe nanocrystals embedded in ZnO thin films using atomic layer deposition
Related Experiment Video
Updated: May 30, 2026

06:50
Synthesis of Hierarchical ZnO/CdSSe Heterostructure Nanotrees
Published on: November 29, 2016
1School of Semiconductor and Chemical Engineering, Chonbuk National University, Jeonju 561-756, Korea.
Nanotechnology
|August 11, 2011
Abstract:
We report the embedding of CdSe/ZnS core-shell nanocrystals into thin films of ZnO grown by atomic layer deposition. Fluorescence from ensembles and that from individual nanocrystals show that the nanocrystal luminescence intensity and stability are preserved through the embedding process. These results are encouraging for the fabrication of optoelectronic nanodevices based on colloidal nanoparticles.