Related Experiment Video
Updated: May 30, 2026

Fabrication of Thin Film Silver/Silver Chloride Electrodes with Finely Controlled Single Layer Silver Chloride
Published on: July 1, 2020
Selective electrodesorption based atomic layer deposition (SEBALD): a novel electrochemical route to deposit metal
M Innocenti1, S Bellandi, E Lastraioli
1Dipartimento di Chimica, Università di Firenze, via della Lastruccia 3, 50019 Sesto Fiorentino (FI), Italy.
Abstract:
The possibility of synergic effects of some metals on the catalytic activity of silver led us to study the way to perform controlled deposition on silver. In fact, many metals of technological interest such as Co, Ni, and Fe cannot be deposited at underpotential on silver, and any attempt to control the deposition at overpotential, even at potentials slightly negative of the Nernst value, did not allow an effective control. However, due to the favorable energy gain involved in the formation of the corresponding sulfides, these metals can be deposited at underpotential on sulfur covered silver. The deposition is surface limited and the successive electrodesorption of sulfur leaves confined clusters of metals. The method can also be used to obtain metal clusters of different size. In fact, the alternate underpotential deposition of elements that form a compound is the basis of the electrochemical atomic layer epitaxy (ECALE), and the reiteration of the basic cycle allows us to obtain sulfide deposits whose thickness increases with the number of cycles. Therefore, the successive selective desorption of sulfur leaves increasing amounts of metals.