Force System with Vertical V-Bends: A 3D In Vitro Assessment of Elastic and Rigid Rectangular Archwires
Published on: July 24, 2018
Deflection load characteristics of laser-welded orthodontic wires
Etsuko Watanabe1, Garrett Stigall, Waleed Elshahawy
1Department of Dental and Biomedical Materials Science, Nagasaki University Graduate School of Biomedical Science, Nagasaki, Japan. ewatana@nagasaki-u.ac.jp
Objective:
To compare the deflection load characteristics of homogeneous and heterogeneous joints made by laser welding using various types of orthodontic wires.
Materials And Methods:
Four kinds of straight orthodontic rectangular wires (0.017 inch × 0.025 inch) were used: stainless-steel (SS), cobalt-chromium-nickel (Co-Cr-Ni), beta-titanium alloy (β-Ti), and nickel-titanium (Ni-Ti). Homogeneous and heterogeneous end-to-end joints (12 mm long each) were made by Nd:YAG laser welding. Two types of welding methods were used: two-point welding and four-point welding. Nonwelded wires were also used as a control. Deflection load (N) was measured by conducting the three-point bending test. The data (n = 5) were statistically analyzed using analysis of variance/Tukey test (P < .05).
Results:
The deflection loads for control wires measured were as follows: SS: 21.7 ± 0.8 N; Co-Cr-Ni: 20.0 ± 0.3 N; β-Ti: 13.9 ± 1.3 N; and Ni-Ti: 6.6 ± 0.4 N. All of the homogeneously welded specimens showed lower deflection loads compared to corresponding control wires and exhibited higher deflection loads compared to heterogeneously welded combinations. For homogeneous combinations, Co-Cr-Ni/Co-Cr-Ni showed a significantly (P < .05) higher deflection load than those of the remaining homogeneously welded groups. In heterogeneous combinations, SS/Co-Cr-Ni and β-Ti/Ni-Ti showed higher deflection loads than those of the remaining heterogeneously welded combinations (significantly higher for SS/Co-Cr-Ni). Significance (P < .01) was shown for the interaction between the two factors (materials combination and welding method). However, no significant difference in deflection load was found between four-point and two-point welding in each homogeneous or heterogeneous combination.
Conclusion:
Heterogeneously laser-welded SS/Co-Cr-Ni and β-Ti/Ni-Ti wires provide a deflection load that is comparable to that of homogeneously welded orthodontic wires.
Related Concept Videos
Deflection of a Beam
Singularity functions, described in an earlier lesson, are powerful mathematical tools that represent discontinuities within a function commonly encountered in structural loading...
Elastic Curve from the Load Distribution
For all beams, the analysis of the beam's reaction to distributed loads begins by understanding the relationship between a beam's load and the resulting shear forces and bending moments. Initially, this...
Deformation of a Beam under Transverse Loading
The insights from the bending moment diagram extend to...
Castigliano's Theorem: Problem Solving
Maximum Deflection
The maximum deflection occurs at a specific point, known as point O, where the tangent to the deflection curve is horizontal. To find point O, the slope of the tangent at any...
Thermal expansion and Thermal stress: Problem Solving
To solve the problem, first, identify the known and unknown quantities. The initial length (L) of the bridge is 1275 m, the coefficient of linear expansion (α) for steel is 12 x 10-6/°C, and the change in temperature (ΔT) is 55 °C.