Determination of γ-γ' lattice misfit in a single-crystal nickel-based superalloy using convergent beam electron

G Brunetti1, A Settefrati, A Hazotte

  • 1Laboratoire d'Etude des Microstructures et de Mécanique des Matériaux (CNRS - UMR 7239), Ile du Saulcy, F-57045 Metz Cedex 01, France.

Micron (Oxford, England : 1993)
|November 8, 2011
PubMed

Related Concept Videos

Determination of Crystal Structures01:29

Determination of Crystal Structures

In the late 1800s, the revelation that light extended beyond visible wavelengths led to the discovery of X-rays by Wilhelm Roentgen. Recognized as high-energy electromagnetic radiation with short wavelengths, X-rays prompted exploration into their interaction with crystals. Max von Laue proposed in 1912 that the periodic arrangement of atoms, ions, or molecules in crystals would cause them to diffract X-rays, a hypothesis confirmed through experiments with copper sulfate and zinc sulfide...
X-ray Crystallography02:18

X-ray Crystallography

The size of the unit cell and the arrangement of atoms in a crystal may be determined from measurements of the diffraction of X-rays by the crystal, termed X-ray crystallography.
Diffraction
Diffraction is the change in the direction of travel experienced by an electromagnetic wave when it encounters a physical barrier whose dimensions are comparable to those of the wavelength of the light. X-rays are electromagnetic radiation with wavelengths about as long as the distance between neighboring...
Precipitation Gravimetry01:03

Precipitation Gravimetry

Precipitation gravimetry is based on converting an analyte into a sparingly soluble precipitate, which is separated by filtration and weighed. An ideal precipitate should be pure, insoluble, of known composition, and easily filtered from the reaction mixture.
In determining nickel by gravimetric analysis, a precipitant of ethanolic dimethylglyoxime is added to a hot nickel salt solution. This is quickly followed by the dropwise addition of dilute ammonia solution until precipitation occurs. A...