Atomic layer deposition synthesis of platinum-tungsten carbide core-shell catalysts for the hydrogen evolution

Irene J Hsu1, Yannick C Kimmel, Xiaoqiang Jiang

  • 1Department of Chemical Engineering, Center for Catalytic Science and Technology, University of Delaware, 150 Academy Street, Newark, DE, USA.

Chemical Communications (Cambridge, England)
|December 14, 2011
PubMed

Related Concept Videos

Heterogeneous Catalysis01:22

Heterogeneous Catalysis

Heterogeneous catalysis involves a catalyst in a different phase from the reactants. It is a process where the catalyst and the reactants are in distinct phases, typically solid and gas or liquid.Most heterogeneous catalysts are metals, metal oxides, or acids. The list includes transition metals like iron (Fe), cobalt (Co), nickel (Ni), palladium (Pd), platinum (Pt), chromium (Cr), manganese (Mn), tungsten (W), silver (Ag), and copper (Cu). These metals possess partially vacant d orbitals that...
Catalysis02:50

Catalysis

The presence of a catalyst affects the rate of a chemical reaction. A catalyst is a substance that can increase the reaction rate without being consumed during the process. A basic comprehension of a catalysts’ role during chemical reactions can be understood from the concept of reaction mechanisms and energy diagrams.
Catalysis01:27

Catalysis

Catalysis influences the rate of chemical reactions by providing an alternative reaction pathway with lower activation energy. A catalyst speeds up a reaction, but it is not consumed during the process. The fundamental principle of catalysis is the ability of a catalyst to alter the reaction mechanism, often introducing a more efficient pathway than the uncatalyzed process.In a catalyzed reaction, the catalyst participates directly in the reaction mechanism. It interacts with reactants to form...
Reduction of Alkenes: Catalytic Hydrogenation02:13

Reduction of Alkenes: Catalytic Hydrogenation

Alkenes undergo reduction by the addition of molecular hydrogen to give alkanes. Because the process generally occurs in the presence of a transition-metal catalyst, the reaction is called catalytic hydrogenation.
Metals like palladium, platinum, and nickel are commonly used in their solid forms — fine powder on an inert surface. As these catalysts remain insoluble in the reaction mixture, they are referred to as heterogeneous catalysts.
The hydrogenation process takes place on the surface of...
Reduction of Alkenes: Asymmetric Catalytic Hydrogenation02:17

Reduction of Alkenes: Asymmetric Catalytic Hydrogenation

Catalytic hydrogenation of alkenes is a transition-metal catalyzed reduction of the double bond using molecular hydrogen to give alkanes. The mode of hydrogen addition follows syn stereochemistry.
The metal catalyst used can be either heterogeneous or homogeneous. When hydrogenation of an alkene generates a chiral center, a pair of enantiomeric products is expected to form. However, an enantiomeric excess of one of the products can be facilitated using an enantioselective reaction or an...