Related Experiment Video
Updated: May 26, 2026

An Optimized Rhizobox Protocol to Visualize Root Growth and Responsiveness to Localized Nutrients
Published on: October 22, 2018
Resistance to compression of weakened roots subjected to different root reconstruction protocols
Lucas Villaça Zogheib1, Guilherme de Siqueira Ferreira Anzaloni Saavedra, Paula Elaine Cardoso
1School of Dentistry, Sagrado Coração University, Bauru, SP, Brazil. lucaszogheib@yahoo.com.br
Objective:
This study evaluated, in vitro, the fracture resistance of human non-vital teeth restored with different reconstruction protocols.
Material And Methods:
Forty human anterior roots of similar shape and dimensions were assigned to four groups (n=10), according to the root reconstruction protocol: Group I (control): non-weakened roots with glass fiber post; Group II: roots with composite resin by incremental technique and glass fiber post; Group III: roots with accessory glass fiber posts and glass fiber post; and Group IV: roots with anatomic glass fiber post technique. Following post cementation and core reconstruction, the roots were embedded in chemically activated acrylic resin and submitted to fracture resistance testing, with a compressive load at an angle of 45º in relation to the long axis of the root at a speed of 0.5 mm/min until fracture. All data were statistically analyzed with bilateral Dunnett's test (α=0.05).
Results:
Group I presented higher mean values of fracture resistance when compared with the three experimental groups, which, in turn, presented similar resistance to fracture among each other. None of the techniques of root reconstruction with intraradicular posts improved root strength, and the incremental technique was suggested as being the most recommendable, since the type of fracture that occurred allowed the remaining dental structure to be repaired.
Conclusion:
The results of this in vitro study suggest that the healthy remaining radicular dentin is more important to increase fracture resistance than the root reconstruction protocol.
Related Concept Videos
Behavior of Concrete Under Compressive Load
As the concrete specimen fractures under...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Bulk Modulus