Related Experiment Video
Updated: May 25, 2026

Functionalization of Single-walled Carbon Nanotubes with Thermo-reversible Block Copolymers and Characterization by Small-angle Neutron Scattering
Published on: June 1, 2016
Polymer binding to carbon nanotubes in aqueous dispersions: residence time on the nanotube surface as obtained by NMR
Anton E Frise1, Guilhem Pagès, Michael Shtein
1Division of Applied Physical Chemistry and Industrial NMR Centre, Department of Chemistry, Teknikringen 30-36, KTH Royal Institute of Technology, SE-10044 Stockholm, Sweden.
Abstract:
The binding of block copolymer Pluronic F-127 in aqueous dispersions of single- (SWCNT) and multiwalled (MWCNT) carbon nanotubes has been studied by pulsed-field-gradient (PFG) (1)H NMR spectroscopy. We show that a major fraction of polymers exist as a free species while a minor fraction is bound to the carbon nanotubes (CNT). The polymers exchange between these two states with residence times on the nanotube surface of 24 ± 5 ms for SWCNT and of 54 ± 11 ms for MWCNT. The CNT concentration in the solution was determined by improved thermal gravimetric analysis (TGA) indicating that the concentration of SWCNT dispersed by F-127 was significantly higher than that for MWCNT. For SWCNT, the area per adsorbed Pluronic F-127 molecule is estimated to be about 40 nm(2).