Effect of chloride ion concentration on the galvanic corrosion of α phase brass by eccrine sweat

Andrew Meekins1, John W Bond, Penelope Chaloner

  • 1Chemistry Division, Department of Chemistry and Biochemistry, University of Sussex, Falmer, Brighton, UK.

Related Concept Videos

Precipitation of Ions03:11

Precipitation of Ions

Predicting Precipitation
The equation that describes the equilibrium between solid calcium carbonate and its solvated ions is:
Precipitation Titration Curve: Analysis01:21

Precipitation Titration Curve: Analysis

The precipitation titration curve demonstrates the change in concentration of one reactant with the volume of titrant added. During the titration of chloride ions with silver nitrate, the precipitation titration curve is divided into three regions: before, at, and after the equivalence point. Before the equivalence point, low redissolution of the sparingly soluble silver chloride precipitate gives a low silver ion concentration. However, in the second region, representing the equivalence point,...
Electrochemical Systems01:24

Electrochemical Systems

Electrochemical systems provide a fascinating insight into the dynamic interplay of charged species within various phases. One notable example is the interaction between a membrane permeable to K⁺ ions but not to Cl⁻ ions, separating an aqueous KCl solution from pure water. As K⁺ ions diffuse through the membrane, they generate net charges on each phase, leading to a potential difference between them.Similarly, when a piece of Zn is immersed in an aqueous ZnSO₄ solution, the Zn metal, composed...
Factors Affecting Solubility04:01

Factors Affecting Solubility

Compared with pure water, the solubility of an ionic compound is less in aqueous solutions containing a common ion (one also produced by dissolution of the ionic compound). This is an example of a phenomenon known as the common ion effect, which is a consequence of the law of mass action that may be explained using Le Chȃtelier’s principle. Consider the dissolution of silver iodide:
Kohlraush’s Law and its Applications01:29

Kohlraush’s Law and its Applications

Kohlrausch's law explains that at infinite dilution, where dissociation is complete, each ion's contribution to the conductivity of the electrolyte is independent of the nature of other ions present in the solution. It also implies that when an electrolyte is highly diluted, the conductance of the electrolyte is the sum of the individual conductances of the ions it generates upon dissociation. The quantity of electricity an ion carries is proportional to its molar ionic conductance, which...
Junction Potentials in Galvanic Cells01:21

Junction Potentials in Galvanic Cells

The Nernst equation, derived under the assumption of thermodynamic equilibrium, calculates the electromotive force (emf) as the sum of potential differences at phase boundaries in a reversible cell without a liquid junction. However, in irreversible cells such as the Daniell cell, an additional potential difference named the liquid-junction potential (EJ) arises across the interface of two electrolyte solutions due to different ion diffusion rates. This EJ represents the potential difference...