Related Experiment Video
Updated: May 24, 2026

Methods of Ex Situ and In Situ Investigations of Structural Transformations: The Case of Crystallization of Metallic Glasses
Published on: June 7, 2018
Glass-transition temperature gradient in nanocomposites: evidence from nuclear magnetic resonance and differential
Aurélie Papon1, Hélène Montes, Mohamed Hanafi
1PPMD-SIMM, Soft Matter Science and Engineering, UMR 7615 CNRS/UPMC/ESPCI ParisTech, Paris, France. aurelie.papon@espci.org
Abstract:
The slowing-down of the dynamics of a polymer chain near a surface has been observed for many years now. Here we show that the behavior of model nanocomposites can be quantitatively described with a gradient of glass-transition temperature. We describe with a single parameter-the range of this gradient-the temperature and solvent effect on the spin relaxation dynamics. Moreover, this parameter allows a quantitative description of the nanocomposite calorimetric response from the one of the bulk polymer.
Related Concept Videos
Atomic Nuclei: Nuclear Spin State Population Distribution
Atomic Spectroscopy: Effects of Temperature
At thermal equilibrium, the relative populations of excited and ground state atoms can be estimated using the Maxwell–Boltzmann distribution. For example, an increase in temperature from...