Evaluation of flexural strength of hipped and presintered zirconia using different estimation methods of Weibull
Bogna Stawarczyk1, Mutlu Ozcan, Albert Trottmann
1Clinic of Fixed and Removable Prosthodontics and Dental Material Science, Center of Dental Medicine, University of Zurich, 8032 Zurich, Switzerland. bogna.stawarczyk@zzm.uzh.ch
Objectives:
This study determined the flexural strength of one hipped and eight presintered zirconia and evaluated the results using different estimation methods of Weibull statistics.
Materials And Methods:
Presintered zirconia specimens were prepared in white state and sintered according to each manufacturer's instructions. One hipped zirconia acted as the control group. The specimens were loaded in a Universal Testing Machine (ISO 6872, 2008). Data were analysed using "normal" (Levene test, one-way ANOVA, Scheffé test) and "Weibull distribution" estimated by either Least Squares (LS) (mean (Excel) and median rank (MINITAB)), Maximum Likelihood (ML) (MINITAB) or ML (MINITAB) with a correction of BS EN 843-5 (2006) (MLC) (alpha=0.05).
Results:
According to normal (σ) and Weibull distribution (s), three-point flexural strength (MPa) of the hipped zirconia (σ=1643 (1507; 1782), s(LS mean rank): 1772, s(LS median rank): 1751 (1619; 1894), s(ML): 1733 (1645; 1826) and s(MLC): (1625; 1848) showed significantly higher results compared to all other presintered zirconia groups (p<0.001). The lowest mean and characteristic strength was observed with GC (σ=817(803;953), s(LS mean rank): 935, s(LS median rank): 935(868; 1007), s(ML): 932(875; 994) and s(MLC): (862; 1009)). The highest Weibull modulus estimated by LS for mean and median rank was observed with LZ (8.9 and 9.8(7.5; 12.9), respectively) and the lowest with ZE (5.1 and 5(3; 8.2), respectively). According to ML and MLC estimation, the control group showed the highest (10.1(6.6; 15.6), 9.2(5.8; 14.2), respectively), and CZ the lowest (5.6(3.8; 8.2), 5.0(3.2; 7.8), respectively) Weibull modulus. No differences in estimates of standard deviations of the normal distribution and the estimates of Weibull moduli for different estimation methods were found between all tested groups.
Conclusions:
Flexural strength of the tested hipped zirconia was higher than those of presintered ones according to both normal and Weibull distribution. LS (median rank) and ML estimates can be compared by a global test and by means of 95% CI. For corrected ML estimates the 95% CI can be interpreted. Estimate calculations in Excel (LS, mean rank) provides information on 95% CI for the Weibull parameters.
Related Concept Videos
Flexural Stress
Hooke's Law states that within the material's elastic limits, stress is directly proportional to strain. In a member experiencing a bending moment, the strain at any point is relative to its distance...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Design of Prismatic Beams for Bending
Bending of Members Made of Several Materials
Hooke's Law determines stress in each material, stating that stress is proportional to strain but varies due to each material's...
Impact Strength of Concrete
Design of Columns under a Centric Load
Euler's formula is applicable under the assumption that the column is a perfect, straight, homogenous prism, and it is operating within the...