Related Experiment Videos
Class II composite resin restorations: a three-year clinical study of six different posterior composites
S A Lundin1, B Andersson, G Koch
1Department of Pedodontics, Postgraduate Dental Education Center, Orebro, Sweden.
Abstract:
Class II restorations of five light-cured posterior composite materials (Occlusion, P 30, Fulfil, Profile and Heliomolar) were followed for three years, and restorations of another material (Distalite) were followed for two years. Twenty-four dentists from The Public Dental Health Service in the county of Bohuslän placed 242 Class II restorations in 213 patients. The restorations were evaluated after three years using the USPHS criteria. Stone casts were used to categorize quantitatively the amount of occlusal wear according to the Leinfelder method. No differences could be found between the different materials regarding clinical properties. The failure rate (USPHS ratings Charlie) was low, 6.5 per cent. The average occlusal wear after three years for most of the materials was about 100 micrometers. Heliomolar showed a better resistance to wear compared with the other materials.