Is the exponent 3/2 justified in analysis of loading curve of pyramidal nanoindentations?
M Troyon1, F Abbès, J A Garcia Guzman
1Laboratoire de Recherche en Nanosciences, EA 4682, Université de Reims Champagne Ardenne, Reims Cedex 2, France. michel.troyon@univ-reims.fr
Abstract:
Kaupp and Naimi-Jamal (2010) claimed that the analysis of published loading curves reveals the exponent 3/2 to the depth for nanoindentations with sharp pyramidal or conical tips. To demonstrate this, they plotted the load vs. the penetration depth to the power 3/2. We show, through examples, the authors' assertion is not credible because the methodology used is misleading and it cannot be asserted that the exponent 3/2 has a universal validity that applies to all kinds of materials.
Related Concept Videos
Generalized Hooke's Law
Three-Dimensional Analysis of Strain
Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity
Eccentric Loading
Residual Stresses in Bending
Euler's Formula for Pin-Ended Columns
To calculate the critical load, envision...