A real time analysis of the self-assembly process using thermal analysis inside the differential scanning calorimeter

Debmalya Roy1, Babita Shastri, K Mukhopadhyay

  • 1Nanoscience and Technology Division, DMSRDE , GT Road, Kanpur, India-208013. debmalya_roy@yahoo.com