Related Experiment Video
Updated: May 19, 2026

Development of a Benchtop Model for Evaluating the Compatibility of Wound Dressing Materials with Negative Pressure Wound Therapy Systems
Published on: May 2, 2025
[The influence of oxygen partial pressure change and vascularization of rabbit wound through negative pressure wound
Fan Yang1, Duan Hu, Xiang-jun Bai
1Department of Traumatic Surgery, the Affiliated Tongji Hospital, Tongji Medical College, Huazhong University of Science and Technology, Wuhan 430030, China.
Objective:
To investigate the effect of vacuum sealing drainage (VSD) on variation of oxygen partial pressure (PtO2) and vascularization.
Methods:
The 12 cases of rabbit's wound models were undergoing the VSD (vacuum group, n = 6) or conventional therapy (conventional group, n = 6). Variation of PtO2 was measured by oxygen partial pressure admeasuring apparatus, expression of hypoxia inducible factor 1α (HIF-1α) mRNA was measured by real-time fluorescent quantitative PCR, content of vascular endothelial growth factor (VEGF) was measured by ELISA after tissue homogenate in 7 days. Vascular endothelial cell (VEC) and new blood capillary (NBC) of hematoxylin-eosin slice of tissue were counted by using light microscope.
Results:
Average value of PtO2 of vacuum group was significant lower than conventional group (t = -99.780 to -5.305, P < 0.01). Expression of HIF-1α (30 minutes, 1, 6, 12 hours were 3.11 ± 0.07, 3.68 ± 0.26, 4.16 ± 0.13 and 3.91 ± 0.26 respectively) and content of VEGF (30 minutes, 1, 6, 12 hours were 103.3 ± 2.4, 134.2 ± 9.0, 167.8 ± 3.8 and 232.1 ± 9.5 respectively) of vacuum group were increased after 30 minutes and significant lower than conventional group (t = 13.038 - 80.208, P < 0.01), and both of them were reduced after 24 hours (P < 0.05). Counting numbers of VEC (2.47 ± 0.45 to 4.70 ± 0.38) and NBC (1.33 ± 0.49 to 4.33 ± 0.68) of vacuum group were increased at the same time-point and significant higher than conventional group (t = -0.670 to 16.500, P < 0.05).
Conclusions:
PtO2 of wound surface could be reduced significantly by VSD. Expression of HIF-1α and content of VEGF were increased by VSD for enhancing differentiated state of VEC and construction of NBC, which were better for vascularization and wound healing.