Related Experiment Video
Updated: May 18, 2026

Using Q Suture to Enhance Resistance to Gap Formation and Tensile Strength of Repaired Flexor Tendons
Published on: June 3, 2020
Effect of gap distance on tensile strength of preceramic base metal solder joints
Farnaz Fattahi1, Milad Motamedi
1Assistant Professor, Department of Prosthodontics, Faculty of Dentistry, Shiraz University of Medical Sciences, Shiraz, Iran.
Background And Aims:
In order to fabricate prostheses with high accuracy and durability, soldering techniques have been introduced to clinical dentistry. However, these prostheses always fail at their solder joints. The purpose of this study was to evaluate the effect of gap distance on the tensile strength of base metal solder joints.
Materials And Methods:
Based on ADA/ISO 9693 specifications for tensile test, 40 specimens were fabricated from a Ni-Cr alloy and cut at the midpoint of 3-mm diameter bar and placed at desired positions by a specially designed device. The specimens were divided into four groups of 10 samples according to the desired solder gap distance: Group1: 0.1mm; Group2: 0.25mm; Group3: 0.5mm; and Group4: 0.75mm. After soldering, specimens were tested for tensile strength by a universal testing machine at a cross-head speed of 0.5mm/min with a preload of 10N.
Results:
The mean tensile strength values of the groups were 162, 307.8, 206.1 and 336.7 MPa, respectively. The group with 0.75-mm gap had the highest and the group with 0.1-mm gap had the lowest tensile strength. Bonferroni test showed that Group1 and Group4 had statistically different values (P=0.023), but the differences between other groups were not sig-nificant at a significance level of 0.05.
Conclusion:
There was no direct relationship between increasing soldering gap distance and tensile strength of the solder joints.
Related Concept Videos
Biasing of Metal-Semiconductor Junctions
In Schottky junctions, where the semiconductor is n-type, applying a positive voltage to the metal relative to the semiconductor reduces its Fermi...
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen also...
Thermal expansion and Thermal stress: Problem Solving
To solve the problem, first, identify the known and unknown quantities. The initial length (L) of the bridge is 1275 m, the coefficient of linear expansion (α) for steel is 12 x 10-6/°C, and the change in temperature (ΔT) is 55 °C.
Relation Between Tensile Strength and Compressive Strength of Concrete
Metal-Semiconductor Junctions
Schottky Barriers
Schottky barriers arise when a metal with a work function (Φm) contacts a semiconductor with a different work function (Φs). Initially, electrons transfer until the Fermi levels of the metal and semiconductor align at equilibrium. For instance, if Φm > Φs, the semiconductor Fermi level is higher than the metal's before contact. The semiconductor's...
Stress-Strain Diagram