Bone properties by nanoindentation in mild and severe osteogenesis imperfecta

Carolyne Albert1, John Jameson, Jeffrey M Toth

  • 1Department of Biomedical Engineering, Marquette University, USA. carolyne.albert@marquette.edu

Abstract

Related Concept Videos

Fractures: Bone Repair01:27

Fractures: Bone Repair

Treatment for a fracture is based on the type of break, the bone affected, and the patient's age.
Minor fractures with no bone displacement are treated by immobilizing the fractured bone using a cast or splint. However, in the case of fractures with displaced bones, the broken bones are repositioned before immobilization to ensure successful healing without deformation and loss of function. The realignment of fractured bone ends is performed through a process called reduction. If the procedure...
Bone Disorders01:29

Bone Disorders

Aging and its effect on bone remodeling is the most common cause of bone disorders. In young and healthy people, bone deposition and resorption happen at an equal rate to maintain optimal bone health.
Bone deposition is also affected by the levels of sex hormones like estrogen and testosterone that promote osteoblast activity and bone matrix synthesis. When the level of these hormones decreases due to aging, it causes a reduction in bone deposition. As a result, bone resorption by osteoclasts...
Compact Bone01:27

Compact Bone

Most bones contain compact and spongy osseous tissue, but their distribution and concentration vary based on the bone's overall function.
Compact bone, also called cortical bone, is the denser, stronger of the two types of bone tissue. It is found under the periosteum and in the diaphyses of long bones, where it provides support and protection. The microscopic structural unit of compact bone is called an osteon, or haversian system. Each osteon is composed of concentric rings of calcified...
Bone Remodeling and Repair01:31

Bone Remodeling and Repair

Osteoclasts are cells responsible for bone resorption and remodeling. They originate from hematopoietic progenitor cells present in the bone marrow. Numerous progenitor cells fuse to form multinucleated cells, each with 10-20 nuclei. A single osteoclast has a diameter of 150 to 200 µM. These cells have ruffled borders that break down the underlying bone tissue and release minerals such as calcium into the blood in bone resorption. Osteoclasts cling to bones with their ruffled edges during bone...
Spongy Bone01:09

Spongy Bone

All bones comprise an outer layer of compact bone, and an interior made up of spongy bone tissue, also called cancellous or trabecular bone. In long bones, spongy bone tissue is mainly found in the interior of the epiphyses (broad ends of the bone).
Spongy bone is more porous, and less dense compared to compact bone. It is composed of concentric lamellae that are arranged irregularly to form the trabecular network. In some bones, the spaces between trabeculae contain red marrow, where...
Bone Formation by Intramembranous Ossification01:29

Bone Formation by Intramembranous Ossification

Intramembranous ossification is one of the two processes involved in the development of bones within an embryo. The flat bones of the face, most of the cranial bones, and the clavicles are formed via this process. During intramembranous ossification, the bones develop directly from sheets of undifferentiated mesenchymal connective tissue.
The process begins when mesenchymal cells in the embryonic skeleton gather together and differentiate into osteogenic cells, which then develop into...