Abstract:
Mode Grüneisen parameters were estimated for α-ZrW(2)O(8) zone-center modes by means of density functional theory calculations and the temperature dependence of the coefficient of thermal expansion was obtained according to the Debye-Einstein model of the quasiharmonic approximation. The lowest energy optic modes were identified at 45 and 46 cm(-1), and were shown to be the main modes responsible for negative thermal expansion at low temperature. Experimental evidence of the lowest energy, triply degenerated infrared active optic mode, was also found in the far infrared spectrum of α-ZrW(2)O(8). Upon increasing temperature, other optic modes with E<25 meV (particularly at 96, 100, 133, 161, and 164 cm(-1)) also contribute significantly to the coefficient of thermal expansion near room temperature. An analysis was made of selected zone-center modes in light of previously proposed models for explaining negative thermal expansion in open framework materials.
Related Concept Videos
Thermal Strain
Thermal expansion and Thermal stress: Problem Solving
To solve the problem, first, identify the known and unknown quantities. The initial length (L) of the bridge is 1275 m, the coefficient of linear expansion (α) for steel is 12 x 10-6/°C, and the change in temperature (ΔT) is 55 °C.
Imperfections in Crystal Structure: Non-Stoichiometric Defects
Crystallographic Point Groups
Imperfections in Crystal Structure: Stoichiometric Point Defects
Theory of Metallic Conduction
In this theory, Newton's second law of motion is used to determine the acceleration of an electron in the presence of an applied electric field. Then, its velocity is expressed via this acceleration.
An electron moves through the crystal, containing positive ions,...