Blends of entirely bio-sourced polymers, namely polylactide (PLA) and starch, have been melt-compounded by lab-scale co-extruder with epoxidized soybean oil (ESO) as a reactive compatibilizer. The starch granules were grafted with the maleic anhydride (MA) to enhance its reactivity with ESO. The ready reactions between the epoxy groups on ESO, the MA groups on MA-grafted starch (MGST) and the end carboxylic acid groups of PLA brought blending components together and formed a compatible compound. An elongation at break (EB) of 140% was obtained in the blend of PLA/MGST/ESO (80/10/10), increased from 5% of a pure PLA. The grafting content of the MA on the starch granules primarily determined the compatibility and properties of the ternary blends, which was also affected by the relative amount of MGST and ESO.
Related Concept Videos
Production of Organic Acids
Preparation of Epoxides
Epoxides result from alkene oxidation, which can be achieved by a) air, b) peroxy acids, c) hypochlorous acids, and d) halohydrin cyclization.
Epoxidation with Peroxy Acids
Epoxidation of alkenes via oxidation with peroxy acids involves the conversion of a carbon–carbon double bond to an epoxide using the oxidizing agent meta-chloroperoxybenzoic acid, commonly known as MCPBA. Since the O–O bond of peroxy acids is very weak, the addition of electrophilic oxygen of peroxy acids to...
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...