Force-degradation pattern of six different orthodontic elastomeric chains
Ah Mirhashemi1, A Saffarshahroudi, A Sodagar
1Assistant Professor, Department of Orthodontics, Faculty of Dentistry, Tehran University of Medical Sciences, Tehran, Iran.
Objective:
An ideal orthodontic force system should exert continuous light force. Thus, many efforts have been made to improve the memory characteristics of elastomeric chains. The aim of this study was to compare elastomeric chains (ECs) claimed by their manufacturers to offer high memory with traditional ones according to their force-extension diagrams.
Materials And Methods:
In this in-vitro study, ECs were divided into six groups, each containing 40 pieces of chain, from three brands (American Orthodontics, GAC and Ortho-Technology). Each brand was divided into two groups with respect to their claimed characteristics (with or without memory). Each sample was stretched to twice its original length and kept constant in 37°C distilled water. Force-extension diagrams were drawn by universal testing machine at 0,1,8,24,72 hours and 1, 2, 4-week intervals. Additionally, the amounts of elongation required to deliver 200 g force were calculated. To compare the results, ANOVA and Tukey tests were performed.
Results:
Force-decay rate was significantly different between traditional and memory chains (p<0.05). For traditional chains, there was a substantial decay in force in the first hour and 30-40% of the force was retained at 4 weeeks. The memory chains demonstrated more constant force and retained 60% of the force. The maximum amount of elongation required to deliver 200 g force belonged to American Orthodontics memory chains (61.9% after 24hr) and the minimum to Ortho-Technology ECs (23.4% initially).
Conclusion:
Memory chains exhibited superior mechanical properties compared to traditional ones. For delivering the same force, memory chains required more elongation. Memory chains of GAC and American Orthodontics showed better characteristics among all chains.
Related Concept Videos
Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity
Circular Shafts - Elastoplastic Materials
As torque on the...
Deformation of Member under Multiple Loadings
In the case of a member with a variable cross-section, the strain is not constant but depends on the position. The deformation of an...
Strain-Energy Density
In the elastic region of a material, the relationship between the stress and the strain is linear and follows Hooke's Law. The strain energy density in this region...
Normal Strain under Axial Loading
Logarithmic Differentiation