Phase discrimination through oxidant selection in low-temperature atomic layer deposition of crystalline iron oxides
Shannon C Riha1, Joy M Racowski, Michael P Lanci
1Materials Science Division, Argonne National Laboratory, Argonne, Illinois 60439, United States.
Abstract:
Control over the oxidation state and crystalline phase of thin-film iron oxides was achieved by low-temperature atomic layer deposition (ALD), utilizing a novel iron precursor, bis(2,4-methylpentadienyl)iron. This low-temperature (T = 120 °C) route to conformal deposition of crystalline Fe3O4 or α-Fe2O3 thin films is determined by the choice of oxygen source selected for the second surface half-reaction. The approach employs ozone to produce fully oxidized α-Fe2O3 or a milder oxidant, H2O2, to generate the Fe(2+)/Fe(3+) spinel, Fe3O4. Both processes show self-limiting surface reactions and deposition rates of at least 0.6 Å/cycle, a significantly high growth rate at such mild conditions. We utilized this process to prepare conformal iron oxide thin films on a porous framework, for which α-Fe2O3 is active for photocatalytic water splitting.