Enhanced band-edge photoluminescence from ZnO-passivated ZnO nanoflowers by atomic layer deposition

Zhi Wei Ai1, Yun Wu, Hao Wu

  • 1Key Laboratory of Artificial Micro- and Nano-structures of Ministry of Education, School of Physics and Technology, Wuhan University, Wuhan 430072, People's Republic of China. H.Wu@whu.edu.cn.

Nanoscale Research Letters
|February 28, 2013
PubMed