Purpose:
The present study aimed to investigate a novel adhesive system containing 0.2% chlorhexidine digluconate (CHX) for its ability to improve the stability of the adhesive interface compared with the use of 2% CHX as a therapeutic primer. Furthermore, the study aimed to confirm the inhibitory properties of these CHX concentrations (0.2% and 2.0%) on dentin matrix metalloproteinase activity by gelatin zymography.
Methods:
Superficial dentin substrate for bonding was obtained from 120 non-carious human molars. A conventional adhesive Peak LC Bond and a CHX-containing adhesive Peak Universal Bond were used either in combination with 35% phosphoric acid (etch-and-rinse approach) or with self-etching primer (self-etch approach) for evaluation of the variables CHX treatment (2.0% therapeutic primer and 0.2% adhesive), adhesive approach (etch-and-rinse and self-etch), and storage time (24 hours and six months). A bonding jig was used to fabricate composite cylinders, which were stored for either 24 hours or six months, after which shear bond strength (SBS) was evaluated using a notched-edge testing device. A three-way analysis of variance and a Student t-test with a significance level of p<0.05 were used to analyze the data. Extracts from concentrated demineralized human dentin powder were subjected to sodium dodecyl sulfate polyacrylamide gel electrophoresis and incubated in the presence of 0.2% and 2.0% CHX.
Results:
No significant effect of CHX treatment, adhesive approach, storage time variables, or their interactions on mean SBS was demonstrated (p<0.05). No significant difference between the control and the CHX-treated groups was detected for either adhesive technique at 24 hours or six months (p<0.05). No significant variation in mean SBS was detected after six months of storage (p<0.05). Zymographic analysis revealed bands of enzymatic activity for the group demineralized with phosphoric acid and complete inhibition of gelatinolytic activity for the groups treated with 0.2% and 2.0% CHX.
Conclusions:
CHX demonstrated inhibition of dentin proteolytic activity. However, when CHX was incorporated into a commercially available adhesive or used as a therapeutic primer, no difference in bond strength was observed at baseline or after six months of storage relative to the control group without CHX.
Related Concept Videos
Bonding and Strength of Aggregate
EDTA: Chemistry and Properties
EDTA: Conditional Formation Constant
For the equilibrium reaction of the metal with the Y4− form of EDTA, the formation...
Complexation Equilibria: The Chelate Effect