SiCN nanofibers with a diameter below 100 nm synthesized via concerted block copolymer formation, microphase separation, and crosslinking
Related Experiment Video
Updated: May 12, 2026

Synthesis of Monodisperse Cylindrical Nanoparticles via Crystallization-driven Self-assembly of Biodegradable Block Copolymers
Published on: June 20, 2019
Saravana K T Pillai1, Winfried P Kretschmer, Christine Denner
1Lehrstuhl Anorganische Chemie II, Universität Bayreuth, Bayreuth, Germany.
Abstract:
SiCN fibers with a mean diameter of 50 nm and an aspect ratio of up to 100 are produced in a two-step process by R. Kempe and co-workers. The key step to fabricate the longitudinal and cross-sectional views of the mesofibers shown here is a concerted block-copolymer synthesis, microphase separation, and cross linking at 140 °C followed by pyrolysis at 1100 °C. Inexpensive components like a commercially available silazane and polyethylene are linked. The fibers may find application in electronic devices, as components of ceramic matrix composites, as fiber beds in high-temperature nano-filtering like diesel fine dust removal, or as thermally robust and chemically inert catalyst supports. Furthermore, the SiCN nanofibers introduced on page 984 are a promising alternative to ultrathin carbon fibers, due to their oxidation resistance.