Solution-Processed, Surface-Engineered, Polycrystalline CdSe-SnSe Exhibiting Low Thermal Conductivity
Published on: May 17, 2024
An experimental apparatus for simultaneously measuring Seebeck coefficient and electrical resistivity from 100 K to
Aiqiang Guan1, Hanfu Wang, Hao Jin
1National Center for Nanoscience and Technology of China, Zhongguancun, Beijing, China.
Abstract:
In this paper, we report a fully automated experimental apparatus for measuring Seebeck coefficient and electrical resistivity of a sample simultaneously in a temperature range of 100-600 K. The Seebeck coefficient is measured using a quasi-steady temperature differential method in which two ceramic heaters are employed to alternately heat the sample. The sample holder is designed to reduce temperature disturbance on its base during a measurement cycle. To demonstrate the accuracy and reliability of the experimental setup, we have performed tests on reference materials including constantan and platinum.
Related Concept Videos
Resistivity
Electrical Conductivity
In a practical conductor, an applied electric field may be sustained, causing a flow of electrons, which produce a current. The differential form of the current, the current density, is related to the electric field.
More generally, it is related to the force per unit charge, which involves the...
Potentiometer
Suppose the emf of a battery needs to be measured. If the battery is directly connected to a standard voltmeter, the measured quantity is...
Applications of EMF Measurements
Wheatstone Bridge
Thus, for accurate resistance measurements, a...
Resistance