Effect of crystallographic orientation on subcritical grain boundary cracking in a conventionally cast

Kameshwaran Swaminathan1, John E Blendell, Kevin P Trumble

  • 1School of Materials Engineering, Purdue University, West Lafayette, IN 47906, USA. kamesh@purdue.edu

Related Concept Videos

Imperfections in Crystal Structure: Non-Stoichiometric Defects01:29

Imperfections in Crystal Structure: Non-Stoichiometric Defects

Non-stoichiometric defects refer to a type of defect in the crystal structure of a compound where the ratio of its constituent elements deviates from the ideal stoichiometric ratio. There are two main types of non-stoichiometric defects: metal excess defects and metal deficiency defects.Metal excess defects occur when there is a slight surplus of metal ions than what is required by the stoichiometric ratio of the compound. For example, heating a sodium chloride crystal in sodium vapor results...
Imperfections in Crystal Structure: Stoichiometric Point Defects01:26

Imperfections in Crystal Structure: Stoichiometric Point Defects

Schottky defects arise when some lattice points in a crystal, such as those in NaCl, remain unoccupied, creating lattice vacancies without disturbing the overall electrical neutrality of the crystal. This defect is common in ionic crystals where the positive and negative ions are similar in size, as seen in sodium chloride and cesium chloride. The presence of Schottky defects enables the crystal to conduct electricity to a small extent through an ionic mechanism. Electric fields cause nearby...
Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
Imperfections in Crystal Structure: Point, Line and Plane Defects01:25

Imperfections in Crystal Structure: Point, Line and Plane Defects

A perfect crystal, in theory, has a uniform structure with the same unit cell and lattice points throughout. However, any deviation from this periodic arrangement is known as an imperfection or defect. These defects can be categorized into three types: point, line, and plane defects.Point defects occur when there is a deviation from the ideal due to missing atoms, displaced atoms, or additional atoms. These imperfections might occur due to imperfect packing during crystallization or because of...
Yield Criteria for Ductile Materials under Plane Stress01:25

Yield Criteria for Ductile Materials under Plane Stress

In designing structural elements and machine parts using ductile materials, it is crucial to ensure that these components withstand applied stresses without yielding. Yielding is initially determined through a tensile test, which evaluates the material's response to uniaxial stress. However, tensile stress is insufficient when components face biaxial or plane stress conditions This condition requires advanced criteria to predict failure.
The Maximum Shearing Stress Criterion, also known as the...
Metallic Solids02:37

Metallic Solids

Metallic solids such as crystals of copper, aluminum, and iron are formed by metal atoms. The structure of metallic crystals is often described as a uniform distribution of atomic nuclei within a “sea” of delocalized electrons. The atoms within such a metallic solid are held together by a unique force known as metallic bonding that gives rise to many useful and varied bulk properties.
All metallic solids exhibit high thermal and electrical conductivity, metallic luster, and malleability. Many...