Related Experiment Video
Updated: May 8, 2026

Physical, Chemical and Biological Characterization of Six Biochars Produced for the Remediation of Contaminated Sites
Published on: November 28, 2014
Pb(II) and Cr(VI) sorption by biochars pyrolyzed from the municipal wastewater sludge under different heating
Weihua Zhang1, Shengyao Mao2, Hao Chen2
1School of Environmental Science and Engineering, Sun Yat-sen University, Guangzhou 510275, China; Environmental Science Division, Oak Ridge National Laboratory, Oak Ridge, TN 37831, USA; Guangdong Provincial Key Laboratory of Environmental Pollution Control and Remediation Technology, Guangzhou 510275, China.
Abstract:
To optimize the pyrolysis process of municipal wastewater sludge for metal sorption, this study investigated the characteristics of the produced biochar under different heating conditions with particular interest in Pb(II) or Cr(VI) sorption. Results indicate that the biochar pyrolyzed at 400 °C for 2 h obtained the largest BET surface area and was rich of organic functional groups, owning the highest Pb(II) (at pH 5.0) and Cr(VI) (at pH 2.0) sorption capacity. The Pb sorption is dominated by the rate-limited chemical processes, and a longer residence during pyrolysis significantly reinforces its sorption bonds. The Cr(VI) sorption is highly pH-dependent, and the optimal occurs at pH 2, where the transformation of Cr(VI) to Cr(III) makes a significant contribution as confirmed by the XPS spectra. Similarly, a longer residence during pyrolysis also facilitates the Cr(VI) sorption in terms of capacity and affinity, likely due to the greater reducing potential of biochar.