Mn(II) deposition on anodes and its effects on capacity fade in spinel lithium manganate-carbon systems
Chun Zhan1, Jun Lu, A Jeremy Kropf
11] Key Laboratory of Organic Optoelectronics and Molecular Engineering, Department of Chemistry, Tsinghua University, Beijing 100084, China [2] Chemical Sciences and Engineering Division, Argonne National Laboratory, Argonne, IL 60439, USA [3].
Abstract:
Dissolution and migration of manganese from cathode lead to severe capacity fading of lithium manganate-carbon cells. Overcoming this major problem requires a better understanding of the mechanisms of manganese dissolution, migration and deposition. Here we apply a variety of advanced analytical methods to study lithium manganate cathodes that are cycled with different anodes. We show that the oxidation state of manganese deposited on the anodes is +2, which differs from the results reported earlier. Our results also indicate that a metathesis reaction between Mn(II) and some species on the solid-electrolyte interphase takes place during the deposition of Mn(II) on the anodes, rather than a reduction reaction that leads to the formation of metallic Mn, as speculated in earlier studies. The concentration of Mn deposited on the anode gradually increases with cycles; this trend is well correlated with the anodes rising impedance and capacity fading of the cell.
More Related Videos
10:41The Effect of Charging and Discharging Lithium Iron Phosphate-graphite Cells at Different Temperatures on Degradation
Published on: July 18, 2018
07:55Elemental-sensitive Detection of the Chemistry in Batteries through Soft X-ray Absorption Spectroscopy and Resonant Inelastic X-ray Scattering
Published on: April 17, 2018
Related Concept Videos
Electrodeposition
Electrodeposition can...
Formation of Complex Ions
MOS Capacitor
The metal gate is typically made from highly conductive materials such as aluminum or polysilicon. Beneath the metal gate lies a thin layer of...