An amperometric hypoxanthine biosensor based on Au@FeNPs for determination of hypoxanthine in meat samples
Rooma Devi1, Sujata Yadav, Renuka Nehra
1Department of Biochemistry, Maharshi Dayanand University, Rohtak 124001, Haryana, India.
Abstract:
A xanthine oxidase (XOD) from buttermilk was immobilized covalently onto boronic acid functionalized gold coated iron nanoparticles (Au@FeNPs) electrodeposited on pencil graphite (PG) electrode, via the boroester linkages, between free hydroxyl groups of boronic acid, α-COOH and -NH2 groups of enzyme. The surface functionalization of Fe/Au nanoparticles with boronic acid (Au@FeNPs) on pencil graphite (PG) electrode was characterized by Fourier transform infrared (FTIR), cyclic voltammetry (CV), scanning electron microscopy (SEM), atomic force microscopy (AFM) and Electrochemical impedance spectroscopy (EIS) before and after immobilization of XOD. The biosensor exhibited optimum response within 3s at pH 7.2 and 30 °C and linearity in the range, 0.05 μM to 150 μM for hypoxanthine with a detection limit of 0.05 μM (S/N=3). Apparent Michaelis Menten constant (Km(app)) for hypoxanthine was 40 μM and Imax 0.125 mA. The biosensor was employed to determine hypoxanthine in fish, chicken, pork, beef meat and lost 50% of its initial activity after its 200 uses over 100 days, when stored at 4 °C.