Layer-controlled, wafer-scale, and conformal synthesis of tungsten disulfide nanosheets using atomic layer deposition
Jeong-Gyu Song1, Jusang Park, Wonseon Lee
1School of Electrical and Electronics Engineering and §Department of Materials Science and Engineering, Yonsei University , Seoul 120-749, Korea.
Abstract:
The synthesis of atomically thin transition-metal disulfides (MS2) with layer controllability and large-area uniformity is an essential requirement for their application in electronic and optical devices. In this work, we describe a process for the synthesis of WS2 nanosheets through the sulfurization of an atomic layer deposition (ALD) WO3 film with systematic layer controllability and wafer-level uniformity. The X-ray photoemission spectroscopy, Raman, and photoluminescence measurements exhibit that the ALD-based WS2 nanosheets have good stoichiometry, clear Raman shift, and bandgap dependence as a function of the number of layers. The electron mobility of the monolayer WS2 measured using a field-effect transistor (FET) with a high-k dielectric gate insulator is shown to be better than that of CVD-grown WS2, and the subthreshold swing is comparable to that of an exfoliated MoS2 FET device. Moreover, by utilizing the high conformality of the ALD process, we have developed a process for the fabrication of WS2 nanotubes.
More Related Videos
10:41Preparation of Liquid-exfoliated Transition Metal Dichalcogenide Nanosheets with Controlled Size and Thickness: A State of the Art Protocol
Published on: December 20, 2016
08:50Preparation of Large-area Vertical 2D Crystal Hetero-structures Through the Sulfurization of Transition Metal Films for Device Fabrication
Published on: November 28, 2017