Poroviscoelastic finite element model including continuous fiber distribution for the simulation of nanoindentation
M Taffetani1, M Griebel2, D Gastaldi1
1Department of Chemistry, Materials and Chemical Engineering, Laboratory of Biological Structure Mechanics (LaBS), Politecnico di Milano, Milano, Italy.
Abstract:
Articular cartilage is a soft hydrated tissue that facilitates proper load transfer in diarthroidal joints. The mechanical properties of articular cartilage derive from its structural and hierarchical organization that, at the micrometric length scale, encompasses three main components: a network of insoluble collagen fibrils, negatively charged macromolecules and a porous extracellular matrix. In this work, a constituent-based constitutive model for the simulation of nanoindentation tests on articular cartilage is presented: it accounts for the multi-constituent, non-linear, porous, and viscous aspects of articular cartilage mechanics. In order to reproduce the articular cartilage response under different loading conditions, the model considers a continuous distribution of collagen fibril orientation, swelling, and depth-dependent mechanical properties. The model's parameters are obtained by fitting published experimental data for the time-dependent response in a stress relaxation unconfined compression test on adult bovine articular cartilage. Then, model validation is obtained by simulating three independent experimental tests: (i) the time-dependent response in a stress relaxation confined compression test, (ii) the drained response of a flat punch indentation test and (iii) the depth-dependence of effective Poisson's ratio in a unconfined compression test. Finally, the validated constitutive model has been used to simulate multiload spherical nanoindentation creep tests. Upon accounting for strain-dependent tissue permeability and intrinsic viscoelastic properties of the collagen network, the model accurately fits the drained and undrained curves and time-dependent creep response. The results show that depth-dependent tissue properties and glycosaminoglycan-induced tissue swelling should be accounted for when simulating indentation experiments.
Related Concept Videos
Elastic Strain Energy for Shearing Stresses
Dynamic Modulus of Elasticity of Concrete
The sonic test is a common method to determine the dynamic modulus. In this test, a concrete beam, sized either 6 x 6 x 30 inches or 4 x 4 x 20 inches, is clamped at its center. Vibrations are initiated at one end of the beam by an electromagnetic exciter unit powered by a...
Circular Shafts - Elastoplastic Materials
As torque on the...
Elastic Strain Energy for Normal Stresses
If...