Iron Nanowire Fabrication by Nano-Porous Anodized Aluminum and its Characterization
Published on: October 6, 2019
Color-tuning method by filling porous alumina membrane using atomic layer deposition based on metal-dielectric-metal
Abstract:
A novel and convenient color-tuning method by filling the porous alumina membrane (PAM) based on metal-dielectric-metal structure is proposed. The pore sizes of PAM as well as the thickness of TiO2 films, deposited by atomic layer deposition, causes various reflection colors due to multilayer interference effects. Overlapping films on top and within the PAM structure can be observed with a scanning electron microscope and will be used to show the change of the effective refractive index of the PAM composite layer. The color-tuning method resulting in changing the dynamics of the PAM layer can be widely applied in fields such as micro-optics, microstructures, nanomaterials, and micro/nanotechnology.
More Related Videos
10:27Simultaneous Multi-surface Anodizations and Stair-like Reverse Biases Detachment of Anodic Aluminum Oxides in Sulfuric and Oxalic Acid Electrolyte
Published on: October 5, 2017
06:30Fabrication of Ultra-thin Color Films with Highly Absorbing Media Using Oblique Angle Deposition