Structure and properties of cotton fabrics treated with functionalized dialdehyde chitosan
Xuemei He1, Ran Tao2, Tianchi Zhou3
1College of Chemistry, Chemical Engineering and Biotechnology, Donghua University, Shanghai 201620, PR China; College of Textiles and Clothing, Yancheng Institute of Technology, Jiangsu 224003, PR China.
Abstract:
In this research, modified cotton fabrics were prepared by pad-dry-cure technique from the aldehyde chitosan solution containing 3-aminopropyltriethoxysilane (APTES) and 1,2-ethanediamine (EDA) respectively. The structural characterization of the modified cotton fabrics was performed by attenuated total reflection ATR, scanning electron microscopy (SEM) and thermogravimetry (TG) analysis and physical mechanical properties were measured. The adsorption kinetics of modified cotton fabrics were also investigated by using the pseudo first-order and pseudo second-order kinetic model. The dyeing rate constant k1, k2 and half adsorption time t1/2 were calculated, respectively. The results show that the mechanical properties of different modified cotton fabrics were improved, and the surface color depth values (K/S), UV index UPF and anti-wrinkle properties were better than those of untreated cotton. Dyeing kinetics data at different temperatures indicate that Direct Pink 12B up-take on the modified cotton fabrics fitted to pseudo second-order kinetic model.