Evaluation of compressive strength of hydraulic silicate-based root-end filling materials
Ryan M Walsh1, Karl F Woodmansey1, Gerald N Glickman1
1Department of Endodontics, Texas A&M University Baylor College of Dentistry, Dallas, Texas.
Introduction:
Hydraulic silicate cements such as mineral trioxide aggregate (MTA) have many clinical advantages. Newer hydraulic silicate materials have been developed that improve on the limitations of mineral trioxide aggregate such as the long setting time and difficult handling characteristics. The purpose of this study was to examine the effect of saline and fetal bovine serum (FBS) on the setting and compressive strength of the following hydraulic silicate cements: ProRoot MTA (white WMTA; Dentsply International, Tulsa Dental Specialties, Johnson City, TN), EndoSequence Root Repair Material (Brasseler USA, Savannah, GA), MTA Plus (MTAP; Avalon Biomed Inc, Bradenton, FL), and QuickSet (QS; Avalon Biomed Inc, Bradenton, FL).
Methods:
Samples of root-end filling materials were compacted into polyethylene molds. Samples were exposed to FBS or saline for 7 days. A universal testing machine was used to determine the compressive strengths.
Results:
QS had significantly lower compressive strength than all other materials (P < .001). White MTA and MTAP mixed with liquid had lower compressive strengths after exposure to FBS compared with saline (P = .003). ERRM, MTAP mixed with gel, and QS were not affected by the exposure to FBS.
Conclusions:
New silicate-based root-end filling materials, other than QS, have compressive strength similar to MTA. Within the limits of this study, premixed materials and those mixed with antiwashout gel maintain their compressive strength when exposed to biological fluids.
More Related Videos
Related Concept Videos
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Mortar Properties
Soundness of Cement
Testing Water Quality
Porosity in Cement Paste
The balance of water to cement in the mix is...
Impact Strength of Concrete