Migration of antimony from polyethylene terephthalate used in mineral water bottles
S Carneado1, E Hernández-Nataren1, J F López-Sánchez1
1Departament de Química Analítica, Universitat de Barcelona, Martí i Franqués, 1-11, 08028 Barcelona, Spain.
Abstract:
The influence of storage time and temperature on Sb migration from PET bottles into mineral water was studied in short-term tests lasting up to 15 days and long-term studies lasting up to 220 days. Samples purchased were stored in three different coloured bottles: clear (CL), light blue (LB) and dark blue (DB). Sb migration was assayed by HG-AFS for total determination and HPLC-ICP-MS for speciation analysis. Migration studies showed that waters stored at 4 and 20 °C were not subject to Sb migration. At 40 °C there was a significant increase in Sb concentration, although the maximum limit established by the European Union (5.0 μgL(-)(1)) was not exceeded, whereas at 60 °C samples were subject to considerable Sb migration after 30 days of storage. In this case, the maximum limit established by the European Union was exceeded and both Sb (V) and Sb (III) were detected.
More Related Videos
05:48Sampling, Identification and Characterization of Microplastics Release from Polypropylene Baby Feeding Bottle during Daily Use
Published on: July 24, 2021
05:05Quantification of Polybutylene Adipate Terephthalate-based Micro- and Nano-plastics from Soil Using Proton Nuclear Magnetic Resonance Spectroscopy
Published on: June 6, 2025
Related Concept Videos
Microbial Bioremediation of Plastics
Bioplastics
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the...