Extremely stable platinum nanoparticles encapsulated in a zirconia nanocage by area-selective atomic layer deposition
Niancai Cheng1, Mohammad Norouzi Banis, Jian Liu
1Department of Mechanical and Materials Engineering, University of Western Ontario, London, Ontario, N6A 5B9, Canada.
Advanced Materials (Deerfield Beach, Fla.)
|November 19, 2014
Abstract:
Encapsulation of Pt nanoparticles (NPs) in a zirconia nanocage by area-selective atomic layer deposition (ALD) can significantly enhance both the Pt stability and activity. Such encapsulated Pt NPs show 10 times more stability than commercial Pt/C catalysts and an oxygen reduction reaction (ORR) activity 6.4 times greater than that of Pt/C.
Keywords:
area-selective atomic layer depositionelectrocatalysisfuel cellsoxygen reduction reactionzirconia nanocages