Elegant design of electrode and electrode/electrolyte interface in lithium-ion batteries by atomic layer deposition
Related Experiment Video
Updated: Apr 19, 2026

Three-electrode Coin Cell Preparation and Electrodeposition Analytics for Lithium-ion Batteries
Published on: May 22, 2018
1Department of Mechanical and Materials Engineering, University of Western Ontario, London, ON, Canada, N6A 5B9.
Abstract:
Lithium-ion batteries (LIBs) are very promising power supply systems for a variety of applications, such as electric vehicles, plug-in hybrid electric vehicles, grid energy storage, and microelectronics. However, to realize these practical applications, many challenges need to be addressed in LIBs, such as power and energy density, cycling lifetime, safety, and cost. Atomic layer deposition (ALD) is emerging as a powerful technique for solving these problems due to its exclusive advantages over other film deposition counterparts. In this review, we summarize the state-of-the-art progresses of employing ALD to design novel nanostructured electrode materials and solid-state electrolytes and to tailor electrode/electrolyte interface by surface coatings in order to prevent unfavorable side reactions and achieve optimal performance of the electrode. Insights into the future research and development of the ALD technique for LIB applications are also discussed. We expect that this review article will provide resourceful information to researchers in both fields of LIBs and ALD and also will stimulate more insightful studies of using ALD for the development of next-generation LIBs.
Related Concept Videos
The Electrical Double Layer
Electrodeposition
Electrodeposition can...
Processes at Electrodes
Electrogravimetric Analysis: Overview
To test the completeness of the...
Ionic Bonding and Electron Transfer
Electrochemical Systems