Comparative evaluation of voids present in conventional and capsulated glass ionomer cements using two different

Mamta Kaushik1, Roshni Sharma1, Pallavi Reddy1

  • 1Department of Conservative Dentistry and Endodontics, Army College of Dental Sciences, Chennapur, CRPF Road, Jai Jawahar Nagar Post, Secunderabad, Andhra Pradesh 500087, India.

Related Concept Videos

Total Voids in Concrete01:12

Total Voids in Concrete

Total voids in concrete encompass gel water volume, capillary pores, and entrapped air. Gel water (retained within the cement hydration products) and physically entrapped or adsorbed water are significant for the hydration process. For complete hydration, it's estimated that the space needed for the products of a cubic centimeter of cement doubles. Capillary pores constitute the unoccupied space within the hydrated cement paste, with their size largely influenced by the water-to-cement...
1.3K
Porosity in Cement Paste01:18

Porosity in Cement Paste

The porosity of concrete is a measure of the void spaces within its structure. These spaces impact its strength and durability significantly. When water and cement interact, a chemical reaction called hydration creates a semi-solid paste. This paste includes combined water, making up approximately 23% of the cement's dry mass, and gel water, which fills minuscule voids known as gel pores, accounting for about 28% of the cement gel volume.
The balance of water to cement in the mix is...
596
Soundness of Cement01:17

Soundness of Cement

The soundness of cement refers to the ability of cement paste to retain its volume after setting. Unsound cement can lead to expansion and structural damage due to the presence of free lime, magnesia, and calcium sulfate. Free lime hydrates very slowly, expanding and causing unsoundness, which is difficult to detect because it intercrystallizes with other compounds. Magnesia also reacts with water, forming crystals that can disrupt the cement's structure. Calcium sulfate can create...
682
Fineness of Cement01:15

Fineness of Cement

The fineness of cement directly influences the rate of hydration, as the hydration begins at the surface of the cement particles. In addition to hydration, the fineness of cement is vital for various properties of concrete including workability, gypsum requirement, and long-term behavior. The fineness of cement is represented in terms of the specific surface of cement which is typically measured in square meters per kilogram, with several methods available for this determination.
Direct...
690
Accelerated Curing of Concrete01:25

Accelerated Curing of Concrete

Accelerating concrete curing is achieved by applying heat and additional moisture. This process accelerates the hydration of the cement, resulting in an earlier strength gain in the concrete. Steam curing is a method wherein the concrete products are either transported through a chamber on a conveyor belt or encased in plastic, allowing steam at atmospheric pressure to circulate freely around them. This process begins with a phase of moist curing that typically lasts between 3 to 5 hours, after...
621
Mortar Joint Deterioration in Masonry01:13

Mortar Joint Deterioration in Masonry

Mortar joint deterioration is a significant concern in masonry structures, with water accumulation in the joints leading to damage from freeze-thaw cycles. The repeated expansion of water during freezing and its melting during thawing develop and propagate cracks in the masonry joints. Eventually, this leads to the spalling of mortar from the joints, loosening masonry units and weakening the structure. The deteriorated mortar joints are also vulnerable to moisture intrusion into the walls.
The...
408