How polymer additives reduce the pour point of hydrocarbon solvents containing wax crystals
Bernard P Binks1, Paul D I Fletcher, Noel A Roberts
1Surfactant & Colloid Group, Department of Chemistry, University of Hull, Hull, HU6 7RX, UK. P.D.Fletcher@hull.ac.uk.
Abstract:
We have investigated how four different pour point depressant (PPD) polymers affect the pour point transition in mixtures of a single pure wax in a solvent. We used either n-eicosane (C20), CH3(CH2)18CH3, n-tetracosane (C24), CH3(CH2)22CH3 or n-hexatriacontane (C36), CH3(CH2)34CH3 as the wax component with either n-heptane or toluene as the solvent component. For all wax-solvent combinations, the measured variation of wax solubility with temperature is well predicted by ideal solution theory. The variation of pour point temperature as a function of the overall wax concentration is quantitatively modelled using the idea that, for each overall wax concentration, the pour point occurs at a temperature at which a critical volume fraction ϕ* of wax crystals has precipitated. Close to the pour point temperature, extraction and examination of the wax crystals show they consist of polydisperse, irregularly-shaped platelets with axial ratios (h/d, where h is the plate thickness and d is the plate long dimension) in the range 0.005-0.05. It is found that the measured ϕ* values corresponding to the pour point transitions are weakly correlated with the wax crystal axial ratios (h/d) for all wax-solvent-PPD polymer combinations. These results indicate that the pour point transition occurs at a volume fraction larger than the value at which the volumes of rotation of the platelet crystals overlap, i.e., 2.5(h/d) < ϕ* < 11(h/d). PPD polymers work, in part, by increasing the wax crystal axial ratio (h/d), thereby increasing ϕ* and reducing the pour point temperature. Since the PPD's ability to modify the wax crystal shape relies on its adsorption to the crystal-solution surface, it is anticipated and observed experimentally that optimum PPD efficacy is correlated with the difference between the wax and the polymer solubility boundary temperatures. This finding and the mechanistic insight gained here provide the basis for a simple and rapid screening test to identify candidate species likely to be effective PPDs for particular wax systems.
Related Concept Videos
Polymer Classification: Crystallinity
Crystalline domains are the regions where polymer chains are aligned in an orderly manner and held together in proximity by intermolecular forces. For example, chains in the crystalline domains of polyethylene and nylon are bound together by van der Waals...
Entropy and Solvation
Plasticizers
Plasticizers function by using surface-active agents to create repulsive electrostatic forces between cement particles. This dispersion enhances the concrete's...
Freezing Point Depression and Boiling Point Elevation
Freezing Point Depression and Boiling Point Elevation
The boiling point of a liquid is the temperature at which its vapor pressure is equal to ambient atmospheric pressure. Since the vapor pressure of a solution is lowered due to the presence of nonvolatile solutes, it stands to reason that the solution’s boiling point will subsequently be increased. Vapor pressure increases with temperature, and so a solution will require a higher temperature than will pure solvent to achieve any given vapor pressure, including one...
Polymers