Abstract:
The aim of this study was to evaluate the effect of adding 10% calcium chloride (CaCl2) on the setting time, solubility and the pH of calcium-enriched mixture (CEM) cement. Setting time was assessed in accordance with American Dental Association specification N°57. Solubility was measured at 24 and 72 h, 7 and 14 days in hydrated and dehydrated conditions by calculating weight change. The pH of MiliQ water in which the CEM cement samples were immersed was measured immediately after each time interval with and without the addition of CaCl2. The data were analysed using the Mann-Whitney U-test and the Student's t-test. The initial setting time was significantly decreased after the addition of 10% CaCl2. The pH of water increased immediately when in contact with the cements in both groups. The weight loss of hydrated and dehydrated specimens was more than 3% and was significantly reduced by the addition of 10% CaCl2.
Related Concept Videos
Hydration of Cement
Effect of Sea Water on Concrete
Concrete in areas between tide marks,...
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
Soundness of Cement
Plasticizers
Plasticizers function by using surface-active agents to create repulsive electrostatic forces between cement particles. This dispersion enhances the concrete's...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...