Abstract:
This in vitro study compared the shear bond strength (SBS) and adhesive remnant index (ARI) of two systems for bonding orthodontic brackets to enamel. The first system involved a self-etching primer (Beauty Ortho Bond, BO) containing surface pre-reacted glass filler. The second involved a primer applied with phosphoric acid etching (Transbond XT, TX). Ninety-six extracted human premolars were divided into eight groups: Group I (TX/direct bonding), Group II (TX/indirect bonding), Group III (BO/direct bonding), and Group IV (BO/indirect bonding). Groups V-VIII were identical to Groups I-IV, respectively, but were also subjected to 1,500 thermal cycles between 5 and 55°C. ARI was scored by binocular microscopy. SBS was analyzed by three-way ANOVA and the Bonferroni test. ARI was analyzed by the chi-squared test. The BO groups showed lower SBS and ARI results than the TX groups. SBS was significantly influenced by the primer material, bonding technique, and thermal cycling.
More Related Videos
07:42Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
08:26Development of Amelogenin-chitosan Hydrogel for In Vitro Enamel Regrowth with a Dense Interface
Published on: July 10, 2014